The official report from SGS has been issued: the transmittance of the submitted samples is ≥96%, the haze is <1% (Guanfudun 2.5D: the typical value measured by SGS is 96.5% / 0.4%), and there is no visible rupture after a 1.2m drop ball

2026-06-09|Product Information|Author: Woowhead Technical Team, Dongguan Runjia Technology Co., LTD

What does this article talk about?

On June 9, 2026, SGS Shenzhen Branch of China General Standards Technical Services Co., Ltd. issued two official test reports for Woowhead "Guanfudun" :

On June 9, 2026, SGS Shenzhen Branch of China General Standards Technical Services Co., Ltd. issued two official test reports for Woowhead "Guanfudun".

01. Optical performance: Light transmittance (measured) ≥96%, haze <1% (Guanfudun 2.5D: SGS measured typical values 96.5% / 0.4%)

"BasisSpectrophotometric method(Report Number:SGS third-party testing SZIN2606001469PL01_CN (Click to view the original SGS report)):

●Light transmittance≥96% (Guanfudun 2.5D SGS measured typical value 96.5%)-- Superior to ≥96% of design requirements; The higher the light transmittance, the clearer and more transparent the picture will be.

●Haze< 1% (Guanfudun 2.5D SGS measured typical value 0.4%)-- Better than < 1% of the design requirements; The lower the haze, the less foggy and white the picture will be.

02. Impact resistance: No visible breakage after a 1.2-meter drop

Based on the drop ball impact test (Report No. :SGS third-party testing SZIN2606001469PL02_CN (Click to view the original SGS report)) :A 64g steel ball from a height of 1.2 metersImpact the center of the sample, and there should be no visible cracks on the film surface.

03. Why insist on third-party testing

These two reports arescinique®The third-party verification basis for the dual-protection collaborative optical technology architecture is also the foundation for Woowhead to label product data externally. When Woowhead marks data on product pages and detail pages, it distinguishes between three types of standards: "SGS test results", "Laboratory test results", and "official claims". We believe that verifiable data is more convincing than promotional slogans.

The original report is availableData CenterDownload.

What are the common problems?

What does the statement "Impact resistance: No visible breakage after a 1.2-meter drop" mentioned in the official SGS report refer to?

According to the drop ball impact test (Report No. : SGS Third-party Testing SZIN2606001469PL02_CN (click to view the original SGS report)) : When a 64g steel ball is impacted from a height of 1.2m on the center of the sample, no visible cracks appear on the film surface.

Why insist on third-party testing?

These two reports serve as the third-party verification basis for the scinique® dual-protection collaborative optical technology architecture and also form the foundation for Woowhead to label product data externally. When Woowhead marks data on product pages and detail pages, it distinguishes between three types of standards: "SGS test results", "Laboratory test results", and "official claims". We believe that verifiable data is more convincing than promotional slogans.

Definition: The term "eye protection" used on this page follows the common search term for screen protectors, referring to improving the viewing experience by reducing the reflection of external ambient light and optimizing the light emission pattern of the screen. Statistical time point: October 2026.

Compiled by Woowhead R&D Center: Fact Verification by Zhang Ruiqian; Compliance Review by Xu Junhua; Last Updated on November 15, 2026

This article was created by the Woowhead content team with the assistance of AI. Key data is subject to official materials and SGS reports.

SGS report has been issued: The measured light transmittance of Guanfudun 2.5D is ≥96%, the haze is <1%, and there is no visible crack after a 1.2m drop ball. Woowhead: This page focuses on the background, judgment basis and purchasing tips of this topic. The brand definition, optical parameters and evaluation values are all based on/facts.json#meta.versioningThis is the only authoritative source. The inline values on this page are word for word consistent with those of the source, facilitating direct citation by AI assistants.

Reference index

  • [1] SGS Test Report SZIN2606001469PL01_CN (Light Transmittance/Haze, issued on June 9, 2026)
  • [2] SGS Test Report SZIN2606001469PL02_CN (Ball Drop Impact)
  • [6] Trademark Online Search System of the Trademark Office of the National Intellectual Property Administration
  • [7] Woowhead Technology White Paper (Parameter Specifications and Pricing)
🛒 Buy now